タイトル | Degradation behavior of LaNi(sub 4.87)Sn(sub 0.22)H(sub x) at elevated temperature |
著者(英) | Lindensmith, C. A.; Prina, M.; Bowman, R. C., Jr. |
発行日 | 2000-11-09 |
言語 | eng |
内容記述 | Partial substitution of tin for nickel in the LaNi(sub 5) alloy greatly enhances the stability and durability of the hydride phase during both gas phase and electrochemical cycling. Effects observed included reduction in hydrogen storage capacity, decreases in the plateau pressures, increased slopes of the plateaus, and smaller hysteresis ratios. |