タイトル | Comparison of high frequency, high temperature core loss and B-H loop characteristics of an 80 Ni-Fe crystalline alloy and two iron-based amorphous alloys |
著者(英) | Schwarze, Gene E.; Wieserman, William R.; Niedra, Janis M. |
著者所属(英) | NASA Lewis Research Center |
発行日 | 1991-01-01 1991 |
言語 | eng |
内容記述 | Limited experimental data exists for the specific core loss and dynamic B-H loops for soft magnetic materials for the combined conditions of high frequency and high temperature. This experimental study investigates the specific core loss and dynamic B-H characteristics of a nickel-iron crystalline magnetic alloy (Supermalloy) and two iron-based amorphous magnetic materials (Metglas 2605S-3A and Metglas 2605SC) over the frequency range of 1-50 kHz and temperature range of 23-300 C under sinusoidal voltage excitation. The effects of maximum magnetic flux density, frequency, and temperature on the specific core loss and on the size and shape of the B-H loops are examined. The Supermalloy and Metglass 2605S-3A and 2605SC data are used to compare the core loss of transformers with identical kVA and voltage ratings. |
NASA分類 | METALLIC MATERIALS |
レポートNO | 93A13882 |
権利 | Copyright |
URI | https://repository.exst.jaxa.jp/dspace/handle/a-is/322385 |
|