| タイトル | Silicon carbide reinforced silicon carbide composite |
| 本文(外部サイト) | http://hdl.handle.net/2060/20080004897 |
| 著者(英) | Lau, Sai-Kwing; Calandra, Salvatore J.; Ohnsorg, Roger W. |
| 著者所属(英) | Saint-Gobain Industrial Ceramics, Inc. |
| 発行日 | 2001-06-12 |
| 言語 | eng |
| 内容記述 | This invention relates to a process comprising the steps of: a) providing a fiber preform comprising a non-oxide ceramic fiber with at least one coating, the coating comprising a coating element selected from the group consisting of carbon, nitrogen, aluminum and titanium, and the fiber having a degradation temperature of between 1400.degree. C. and 1450.degree. C., b) impregnating the preform with a slurry comprising silicon carbide particles and between 0.1 wt % and 3 wt % added carbon c) providing a cover mix comprising: i) an alloy comprising a metallic infiltrant and the coating element, and ii) a resin, d) placing the cover mix on at least a portion of the surface of the porous silicon carbide body, e) heating the cover mix to a temperature between 1410.degree. C. and 1450.degree. C. to melt the alloy, and f) infiltrating the fiber preform with the melted alloy for a time period of between 15 minutes and 240 minutes, to produce a ceramic fiber reinforced ceramic composite. |
| NASA分類 | Nonmetallic Materials |
| 権利 | No Copyright |
|